HCHL was referring to per cell, not the pack, with the 1.2v number. (7.2v for a typical 6 cell pack)
Yes, typical discharge under load is to 0.9v per cell (5.4v for 6). But a good cell will rebound after being removed from the load, back up to the ~1.2v per range.