R/C Tech Forums - View Single Post - Tamiya TRF419
Thread: Tamiya TRF419
View Single Post
Old 01-11-2015 | 05:11 PM
  #744  
niznai's Avatar
niznai
Tech Elite
 
Joined: Feb 2009
Posts: 2,972
From: All over the place
Default

The (plain/blue anodised) Aluminium (or steel) ballstuds are a fraction smaller than the fluorine coated ball ends hence a little loose in the cups. The fluorine coated are perfect (no play, whilst free to move). Maybe the fluorine coating makes the difference.
niznai is offline