Is it true that the Aluminium Sleeve wear out more than Bass Sleeve? That why only Mega release only Evo6 Bass Sleeve??
|
Re: About Nitro AAC engine
Originally posted by Slideng Is it true that the Aluminium Sleeve wear out more than Bass Sleeve? That why only Mega release only Evo6 Bass Sleeve?? No it is not true. Base material of sleeve realy doesn't metter on wear, because it is coated by Chrome, the piston-is the part which is wearing out. If chrome plating done well, you can changed piston in the same sleeve many times-4-5 times at list and then you have to correct tapering little bit in sleeve and it is good to go for 5 more pistons. |